I'm planning on painting a new birch kitchen bookcase using Benjamin Moore alkyd high gloss enamel in white.The Moore spec sheet states that all alkyd based paints experience some degree of yellowing and that I should be using latex based paints instead. From my experience latex will not produce the same smooth high gloss as oil. I've contacted Benjamin Moore asking what they consider "some degree of yellowing" to be but have not gotten a reply. Anyone have any info on the yellowing or latex gloss question?

Comments (9)

  • 16 years ago

    It yellows over time because of the solvents used in the oil based products. It depends on how much sunlight the object you have painted gets...less sunlight, it will yellow faster. This is normal with all oil based paints. It's also true that high gloss latex just isn't the same as high gloss oil unless you spray it. I would suggest a semi-gloss in latex unless you really want that high shine, then you pretty much have to use oil.

  • 16 years ago

    Paintguy; thanks for your response. The kitchen is brightly lit with two walls of windows from countertop to ceiling, but no direct sunlight to speak of. I'm curious about the term-yellowing. Is it a slight shift towards a cream color or a real nasty yellow? A slight shift might be o.k.considering the smooth gloss finish.

  • 16 years ago

    Well, some people notice the yellowing and some do not. If your room is well lit, that will help. It will not yellow as quickly as the inside of a closet. The yellowing is not really a pleasant look....it makes the trim look dirty IMO, almost like someone blew cigarette smoke on it repeatedly. Also, it does not yellow uniformly....some areas get more yellow than others.

  • PRO
    16 years ago

    It doesn't yellow uniformly should be emphasized. I actually thought my dog pee'd on the wall in one spot in particular in my hallway. Turns out it's just where the paint color is starting to turn. Wish I didn't have oil, but I do. I don't even know what oil-based paint was used as the doors and millwork were sprayed in Juarez, MX. All the cabinetry in the house was built in Juarez too. We seemed to have missed most of the major off gassing since the house sat vacant for a while so I think we'll be fine, but I could have done without the life-long yellowing issues.

  • 16 years ago

    Hi,
    It's the alkyd resin medium of oil enamel that incurs the yellowing. It's the same substance and process that causes oil varnish to darken over time. The color affect is best described as "ambering" IMO.
    I have an interesting manifestation of yellowing occurring in my new (2007) kitchen remodel. I painted the moldings above my cabinets in a color called Cloth, which is an off-white with yellow oxide, black and gray. So it was not any concern that yellowing would really affect the color. The ceiling I painted in the same tint, but in an eggshell acrylic latex. I have touched up both paints, and it's only the ceiling that has yellowed, not the satin Impervo oil. So, there you have it. Acrylic doesn't guarantee freedom from yellowing, nor is it a given that oil enamel will yellow in a short time.
    Casey

  • PRO
    16 years ago

    Well, the latex did not yellow from a chemical change, it may not be the same color as it was when applied but that is from being old and dirty not form a chemical change.The oil will change eventually, there is no arguing that fact.

  • 16 years ago

    Thanks all for your invaluable help. I'll pass on the oil and go with BM latex Impervo.

  • 16 years ago

    Just one more tip if your still there. I would not use a latex paint for kitchen cabinets. The type of paint you should use is alkyd urethane waterbased for better adhesion, durability, finished apperance,and non yellowing. If BM Impervo is a latex, don't use it. You don't need an oil based paint. There are several companies that make FPE equivalent paint according to government specs. One of them is ICI Dulux, the brand I use. Whatever you use, just be sure it's alkyd, urethane, waterbased.